Package Size: 0
Reference Number:
- 1
Prepare
Ensure the resin is stored at room temperature and protected from light. Stir prior to use.
- 2
Print
Use DLP, LCD, or SLA printing technology. Ensure print settings match resin requirements.
Suggested Devices:
- SLA
- DLP
- LCD
- 3
Wash
Rinse printed items with IPA or ethanol to clean residues.
- 4
Post-cure
Expose to UV light for 2 x 30 min to fully cure the printed parts.
Suggested Devices:
- UV Post-Cure Devices
- 5
Mold Removal
Submerge in water or diluted alkalic media for mold removal post-injection.
| Property | Value | Unit | Test Condition |
|---|---|---|---|
| Tensile Strength | 46 | MPa | |
| Tensile Modulus | 2100 | MPa | |
| Elongation at Break | 13 | % | |
| Shore hardness | 82 | D | |
| Viscosity | 40 | mPa.s | @ 25 °C |
| Density | 1.11 | g/mL | |
| Critical Energy 385 nm (Ec) | 0.8 | mJ/cm2 | |
| Depth of Penetration 385 nm | 0.12 | mm | |
| Detergent | Isopropyl alcohol OTHER | ||
| Printing Technology | SLA DLP LCD |